US10837130B2
University of Texas System
The described incandescent tension annealing processes involve thermally annealing twisted or coiled carbon nanotube (CNT) yarns at high-temperatures (1000° C. to 3000° C.) while these yarns are under tensile loads. These processes can be used for increasing yarn modulus and strength and for …